Polyurethane self-skinning foam, also known as whole skin molded foam, is called “integral skin foam” (referred to as ISF) in English. It is different from general polyurethane semi-rigid foam. Polyurethane semi-rigid foam usually uses ABS or PVC as the surface material, which is filled with polyurethane semi-rigid foam, which becomes a kind of sandwich material like “sandwich”; polyurethane self-skin foam does not use other plastics as surface material, special use The process produces a polyurethane component with a solid outer skin at a time. Its outer skin is thicker, between a few tenths of a millimeter and 2.3 millimeters. The density of the outer skin is generally 1000-1200Kg/m3, while the density of the core layer is several hundred Kg/m3.
Polyol | Milky white viscous liquid |
Isocyanate | Yellow brown liquid |
Material temperature | 25±2 ℃ |
Ratio (A:B) | 100:40±2 |
Crean Time | 14±3 s |
Viscosity (mPas) | 1000±150 |
150±50 | |
Mold Temperature | 55±5 ℃ |
Molding Time | 240±20 s |
Gel Time | 55±5 s |
Free Rise Core Density | 80±10 kg/m³ |